| brightness | 
| 89% per TAPPI T-452 Test Method |  | 
| Roll dimensions |  | 
| Roll dimensions |  | 
| Printing material dry time | 
| Less than 10 minutes (@23ºC, 50% RH) |  | 
| Media finish |  | 
| Printing material gloss level | 
| High-gloss per ASTM D-523 Test Method |  | 
| Printing material lamination | 
| Yes, hot or cold lamination. |  | 
| Fade-resistance note (indoor home or office) | 
| Indoor, Display permanence rating for interior displays/away from direct sunlight, under glass by HP Image Permanence Lab and/or by Wilhelm Imaging Research, Inc. For details: http://www.hp.com/go/supplies/printpermanence |  | 
| Fade-resistance (indoor commercial window, dye ink) |  | 
| Fade-resistance (indoor home or office, dye ink) | 
| 2.6 years (tested under glass) |  | 
| Fade-resistance (indoor home or office, pigment ink) | 
| 30+ years with HP 83 UV pigment inks |  | 
| Opacity | 
| 95% per TAPPI T-425 Test Method |  | 
| Primary material | 
| Wood fiber and Polyethylene |  | 
| Shelf life | 
| 2 years, unopened in original packaging |  | 
| Smoothness | 
| 10 per TAPPI T-538 Test Method |  | 
| Printing material thickness | 
| 6.6 mil/168 microns per ISO 534 Test Method |  | 
| Printing material waterfastness | 
| Lamination required for dye inks; testing ongoing for UV inks |  | 
| Print material weight | 
| 190 g/m² per ISO 536 Test Method |  | 
| Whiteness | 
| 105 per CIE Ganz 82 Test Method |  | 